Metal-ceramic crown: aesthetic budget dental prosthetics


Reasons for chipping ceramics in metal-ceramic structures

At the junction of the metal frame of the denture and the ceramic coating, strong stresses often arise, which in stressful situations lead to the formation of cracks, chips or spalls in the ceramics.

The main reasons for ceramic chipping are:

  • Mismatch between the thermal expansion coefficients of ceramics and the metal alloy from which the frame is made.
  • Unreasonable choice of metal ceramics as a material for a fixed prosthesis in some patients (for example, those suffering from bruxism).
  • If the intermediate part of a metal-ceramic bridge is too long, the frame of which is made of precious alloys (which have lower rigidity than non-precious alloys), chewing loads on it can lead to chipping of the veneer.
  • Incorrect tooth preparation, for example, insufficient taper, can lead to stress in the framework of the metal-ceramic crown and subsequent chipping of the veneer.
  • Chips often occur when performing orthopedic work (especially large-scale ones) without an articulator and a facebow.
  • When fixing a metal-ceramic prosthesis with excessively thick cement, or when foreign bodies get between the tooth stump and the crown.
  • Chips may be a consequence of incorrect modeling of the metal-ceramic frame of the future prosthesis:

- insufficient height of the frame, which necessitates the layering of an excessive amount of ceramics - unmodeled tooth relief - non-compliance with the technology of mechanical and chemical processing of the metal frame - holes in the metal frame, which technicians close with ceramics. Subsequently, after cementing the crowns, tension arises here, since the cement presses evenly on all walls and later a chip forms in this place and rapid decementing of the structure.

If you have a problem similar to that described in this article, be sure to contact our specialists. Don't diagnose yourself!

Why you should call us now:

  • We will answer all your questions in 3 minutes
  • Free consultation
  • The average work experience of doctors is 12 years
  • Convenient location of clinics

Single contact phone number: +7

Make an appointment

  • The cause of chipping may be stress in the ceramics or metal frame, resulting from non-compliance with technological rules for working with ceramics:

- overheating of the metal during firing of ceramics - violation of temperature relationships during successive firing and cooling of ceramics - violation of the rules for working with ceramic masses offered by manufacturers - non-compliance with ceramic processing technology.

  • Careless or careless handling of the patient with prosthetic metal-ceramic structures. The fragility of ceramics under inadequate loads, and less often during sudden temperature changes, should be taken into account. We also recommend that you read the article about installing ceramic crowns at 32Dent dentistry.

Technological aspects of metal ceramics

In the process of manufacturing metal-ceramic structures, there are a number of key points that deserve special attention.

Tooth preparation for metal ceramics.

  • The tooth must be prepared (ground) with a ledge at the gum level.
  • The total thickness of the metal frame and the ceramic mass covering it is about 1.5 mm. As a result, if the tooth is ground without a ledge, we get the edge of the crown hanging over the gum and pressing on it. The crown presses against the blood vessels and a “bruise” forms. The metal frame comes into direct contact with the gum, and metal ions cause it to darken.
  • In the case of preparation with a shoulder, the edge of the metal-ceramic crown rests on the hard tissues of the tooth without injuring the mucous membrane. This technology is quite labor-intensive, and its implementation requires a modern dental unit and, of course, the qualifications of a doctor and dental technician.

The intermediate part of the metal-ceramic bridge prosthesis should also not put pressure on the mucous membrane (gum), otherwise bedsores may form. Of course, in those places where it is visible, you have to make a compromise, but in any case the touch should be very gentle. And if food gets into a place where there is a loose seal, it will be much easier to remove it from there than in the case of the “full contact” option.

Many doctors “sin” by depulping (removing the nerve of the tooth) even healthy teeth under metal-ceramics, which is not always justified, since modern technologies make it possible in many cases to avoid this procedure. Depulped (dead) teeth cannot resist infection and often have to be re-treated. In addition, a pulpless tooth becomes more fragile and can collapse under a heavy metal-ceramic structure.

Types of crowns

To restore severely damaged or completely lost teeth, dentists at the Beryozka clinic offer metal-ceramic dental crowns in several varieties.

Traditional products

For the manufacture of classic crowns, alloys of chromium and cobalt are usually used. The materials are inexpensive and make very durable foundations. But there is one nuance - the frame part is not completely processed with ceramic mass, so there remains a small gap at the junction of the prosthesis with the gum. As a result, the metal comes into contact with soft tissues and an unsightly bluish tint forms on the gums.

If you make a prosthesis with shoulder mass, you can avoid the negative effect. Such structures are completely covered with a ceramic layer, but the manufacturing cost will be more expensive than usual.

Structures with a frame made of precious metals


If you use precious metals to make a frame base, then such structures are more aesthetic and durable. Considering that the most important part of the structure is the frame, to achieve maximum quality the best solution would be to use noble metals for its manufacture.

Crowns using computer technology

When creating prostheses using this technique, the frame is not made by casting, but using a special milling machine. Such structures adhere perfectly to the surfaces of natural teeth, which significantly increases their strength characteristics.

Computer modeling allows you to design structures for each clinical case with maximum accuracy and achieve the highest results in reliability and aesthetics.

Stages of manufacturing a metal-ceramic bridge prosthesis

The main indication for prosthetics using fixed bridges is the absence of one or more teeth.

If you have a problem similar to that described in this article, be sure to contact our specialists. Don't diagnose yourself!

Why you should call us now:

  • We will answer all your questions in 3 minutes
  • Free consultation
  • The average work experience of doctors is 12 years
  • Convenient location of clinics

Single contact phone number: +7

Make an appointment

Dental prosthetics using fixed metal-ceramic prostheses is one of the most common methods of treating violations of the integrity of the dentition and restoring chewing function. For this purpose, missing teeth are replaced with artificial ones, supported by adjacent teeth. The functional basis of such treatment is the reserve capacity of the dentition, which allows it to withstand additional load.

A fixed metal-ceramic bridge prosthesis is a structure consisting of one or more artificial (metal-ceramic) teeth rigidly attached to adjacent natural teeth using fixing elements - metal-ceramic crowns.

Typically, the number of supports in a bridge is two, but sometimes there is a need for three or more supports. Due to the fact that the supporting teeth experience pressure not only directly on them, but also on the intermediate part of the bridge, the number of replaced teeth cannot be too large. As a rule, this is 1-2 teeth.

The manufacturing process of a metal-ceramic bridge consists of clinical and laboratory stages.

Clinical stage

After the examination, if necessary, preliminary treatment is carried out: gum treatment, filling of supporting teeth and, if this is unavoidable, removal of the pulp and filling of root canals.

Then the teeth are prepared, on which the crowns that are part of the metal-ceramic bridge will be placed. This stage consists of grinding down their convex surfaces that prevent the crown from being put on.

After processing the teeth, an impression is taken and a plaster model of the missing dentition, along with data on the state of the bite, is sent to the dental laboratory.

Laboratory stage

In the laboratory, jaw models are made, on which the frame of the bridge is formed from wax, and then the metal frame is cast in a foundry.

Then the frame can be coated with a golden sublayer, which, due to the high gold content, allows the ceramic mass to be applied in an ultra-thin layer, through which the black or dark gray color of the oxide film covering the surface of the metal frame will not show through.

Next, the frame is covered with ceramic mass. The ceramic coating is applied in layers in accordance with the colors selected by the orthopedic surgeon. The “face bow” data is transferred to the articulator and the bridge is finally modeled in shape, taking into account the bite and relationship of the teeth during movement.

A bridge is a rather complex structure, so another intermediate visit is required - fitting of the frame. During the third visit, the final correction is made. The ceramics are covered with glaze, which gives the prosthesis a natural look, and with the help of special cement, the metal-ceramic prosthesis is fixed to the teeth.

What is a metal-ceramic crown?

A “metal-ceramics” dental crown is an orthopedic structure consisting of a durable metal frame base, coated on the outside with a finishing layer of special dental ceramics.

The base is made of different metal alloys: titanium, nickel, gold and others. The ceramic coating is applied to the frame in layers, with each layer subjected to heat treatment. This technique ensures super-strong adhesion of the ceramic composition to the metal base.

Stages of manufacturing a metal-ceramic crown

The traditional manufacturing process of metal-ceramic crowns involves the following steps:

  • Determination of tooth color, characteristic features, structure of enamel, dentin, determination of the transparent layer, the presence of individual characteristics (enamel cracks, staining of fissures in the chewing group of teeth, the presence of chalky stains, enamel abrasion, etc.).
  • Next comes the removal of the destroyed dental tissue and the process of preparation (grinding) of the tooth, which takes a very long time. In order to ensure that after installing a metal-ceramic crown there is no effect of the so-called “blue” gum or compression of the gingival dental papilla by the crown, the doctor must very carefully grind the tooth to create a gingival ledge (the angle on which the crown will rest). Only with this method will the work be successful.
  • An impression is then taken and sent to the laboratory.

During the production of permanent metal-ceramic structures, a temporary crown is placed, which hides the defect and eliminates psychological discomfort.

  • After the metal frame is made, ceramic masses are applied to it layer by layer, recreating natural teeth as accurately as possible. Next comes the artistic design of the metal-ceramic crown, taking into account the individual characteristics of the tooth.
  • Then follows the fitting of an almost finished metal-ceramic crown (a metal frame with ceramics already applied, but not glazed). At this stage, the color of the crown is finally determined, because You can still make changes.

Finally, at the last visit, the permanent crown is placed. The entire process of manufacturing a metal-ceramic crown takes on average up to 10 working days.

Examples of work by Berezka dentists before and after crown installation

The Berezka dental clinic offers different options for prosthetics with metal-ceramic crowns depending on the condition of the patients’ teeth. But regardless of the type of structure and technology for installing the prosthesis, the emphasis is on the exceptional quality of orthopedic products.

Our clinic’s specialists use metal ceramics from leading brands, which are characterized by maximum wear resistance and safety.

In the photo below you can see examples that depict different clinical pictures of the installation of prostheses and see the professionalism of our orthopedic doctors.

Materials used in metal ceramics

In metal-ceramics, a metal frame is used as a base, which solved the problems of excessive fragility of ceramics. Ceramic is applied layer by layer to the outer surface of the metal and held firmly in place by sintering. As a result, a metal-ceramic crown is reliable, durable and very beautiful. Plus, it looks like a real healthy tooth.

To effectively protect teeth from destruction under crowns, teeth are treated with a protective paste that releases fluoride into the tooth tissue. Modern dental cements are used to fix metal-ceramics, which makes it possible to achieve the strongest fixation. A high-quality metal-ceramic structure lasts for decades. The average service life of cermets on base alloys is 10-12 years. On gold-platinum alloy 15 years or more.

Indications for installation of metal ceramics

Dentists install crowns and bridges made of metal-ceramics in case of functional, anatomical or aesthetic inferiority of natural teeth.

The main indications for use include:

  • destruction of natural crowns due to carious processes or traumatic factors, in which restoration with inlays or fillings is impossible;
  • increased abrasion of tooth enamel;
  • abnormalities in the development or incorrect position of the front teeth and other methods do not provide the desired effect in eliminating such anomalies;
  • wedge-shaped defects of teeth in the smile area and fluorosis;
  • changes in the color of tooth enamel and the inability to achieve whiteness using whitening technologies;
  • absence of one or more units in the dentition;
  • inconsistency of existing orthopedic structures in terms of functionality and aesthetics.

In some cases, metal-ceramic products are used for mild and moderate periodontitis as splinting structures.

Ceramic lining in metal ceramics

The quality of a metal-ceramic prosthesis depends on many factors. Color accuracy is determined mainly by the quality of the ceramic mass. Imported ceramics convey color more accurately than domestic ones; in addition, they are more stable during processing and use - they do not change color when fired, and do not crack.

If you have a problem similar to that described in this article, be sure to contact our specialists. Don't diagnose yourself!

Why you should call us now:

  • We will answer all your questions in 3 minutes
  • Free consultation
  • The average work experience of doctors is 12 years
  • Convenient location of clinics

Single contact phone number: +7

Make an appointment

Applying porcelain mass to a metal frame is a long and painstaking job, since it is applied in layers and after each application the mass is fired in a special vacuum oven. Firing metal ceramics is a very important task. If the temperature or barometric modes are chosen incorrectly, the ceramics will crack and all the work will have to be done again. It is thanks to the layered application of porcelain that metal-ceramic teeth accurately convey the color and transparency of natural teeth. In addition, porcelain is intertwined with the tissues of the oral cavity and is hygienic.

Recently, ceramics have appeared in world dental practice, having a rigidity coefficient comparable to that of healthy teeth, which makes it possible not to injure or abrade antagonist teeth when chewing.

The use of the latest technologies allows you to give metal ceramics any color. Typically, the color of metal-ceramics is as close as possible to the color of the patient’s teeth. To do this, doctors use a set of small porcelain plates in the shape of a tooth (each plate has its own shade); Dentists call such sets a “color chart.” Depending on the specific situation, a metal-ceramic crown can be made so that porcelain covers only certain sides of it that are visible when smiling and talking, and the remaining parts of the crown are made completely metal.

The world leaders in the production of dental ceramics and porcelain are Ducera, Noritake.

One of the leading factors when choosing porcelain for ceramic cladding is the constancy of its coefficient of thermal expansion, which prevents the occurrence of cracks in the ceramic coating even during the manufacture of extended multi-unit structures. Some manufacturing companies produce porcelain, the coefficient of thermal expansion of which does not change during multiple firings, and is also little sensitive to the selected firing mode, therefore metal-ceramic products coated with such porcelain can be successfully fired in any dental furnace, starting from the simplest ones with a strictly specified heating rate , and ending with ultra-modern ones.

Another important criterion for choosing porcelain for metal-ceramic dentures is its strength. According to the international standard ISO 9693 “Dental metal-ceramics for dental prosthetics,” the flexural strength of porcelain must be at least 50 MPa.

Another pleasant distinguishing feature of some types of porcelain is their resistance to greening when applied to metal frames made of semi-precious silver-based alloys.

Manufacturing process

Patients who want to install truly high-quality metal-ceramic dentures should understand that this will not be possible quickly. It will take at least 10-14 days to produce them. The procedure for making crowns is as follows:

  • The doctor applies a special mixture to the already ground teeth, which hardens almost instantly. After removing it, the dentist takes an impression;
  • if the impression is made successfully, then it serves as the basis for creating a plaster model of the tooth being restored;
  • Next, a model of a metal frame made of wax is developed. The finished model is transferred to a dental prosthetic workshop for the manufacture of a prosthesis from an alloy agreed with the patient;
  • When the frame is completed, fitting is required. It is put on the patient’s teeth and if all is well, it is returned to the technicians;
  • in the workshop, a ceramic composition is applied to the frame in two layers and sent to a specialized oven for heat treatment;
  • then enamel is applied to the product, corresponding to the shade of the patient’s natural tooth covering;
  • The orthopedist performs a control fitting. When the crown fits snugly and meets all the requirements, it is sent to the workshop again. There, a special glaze is applied to the prosthesis to add shine and the final firing is performed.

Only after all the above steps are the crowns considered ready for installation. If some specialists offer you shorter terms for making crowns, then this is a serious reason to doubt the quality of the products and the professionalism of the doctors themselves.

Types of alloys in metal ceramics

Gold-platinum alloy

The classic version with which orthopedic dentistry began. The first crowns were made from gold at the end of the 19th century.

Nowadays, many materials have appeared that, along with solving the problem of restoring chewing function, are quite durable and at the same time meet high aesthetic and cosmetic requirements. But gold, as a material for the manufacture of frames for metal-ceramic prostheses, is still relevant today.

Only a noble alloy can adhere so precisely to the treated tooth, which practically eliminates disintegration and recurrent caries. Gold almost never causes allergies.

The disadvantage of using a gold alloy is the limitation on the length of the intermediate (located between two supports) part of the metal-ceramic bridge (in the manufacture of metal-ceramic bridges), as well as the price: the cost of such a crown is from 10,000 rubles.

Sometimes, to improve color rendition, on a metal frame cast from other metals. a thin layer of gold is applied, which illuminates through a layer of ceramic mass with a warm yellowish color.

Nickel alloy

Most often, nickel-based alloys are used to cast the frame, which is the most accessible of the metals that can be the basis for metal-ceramics. With nickel alloys there are no problems when casting and fitting in the patient's mouth.

However, despite all the advantages, nickel has a serious drawback. This metal is a strong allergen.

Our body's daily need for nickel is thousandths of a gram, and the production of one metal-ceramic crown requires 2 grams of an alloy containing 1.3 grams of nickel. Thus, the metal is in contact around the clock with the oral mucosa, tooth tissues, and jaw. The result is allergic reactions and weakened immunity.

In Germany, they abandoned the use of nickel in dental prosthetics 10 years ago (as well as stainless steel back in the 30s).

If you have a problem similar to that described in this article, be sure to contact our specialists. Don't diagnose yourself!

Why you should call us now:

  • We will answer all your questions in 3 minutes
  • Free consultation
  • The average work experience of doctors is 12 years
  • Convenient location of clinics

Single contact phone number: +7

Make an appointment

Cobalt-chromium alloys

The most optimal option taking into account biocompatibility and cost.

In cost, they are only 1.6 times more expensive than allergenic nickel alloys. The biocompatibility of the cobalt alloy is 36% (for the gold-platinum alloy it is 42%, and only one’s own teeth are 100% biocompatible), they are non-toxic and do not cause allergic reactions. Cobalt alloys are durable, and metal-ceramic bridges of fairly long length can be made from them.

Chromium alloys are not dangerous; only some of its salts are poisonous, but they cannot form in the oral cavity.

Molybdenum

A non-toxic metal, it is added to dental alloys in very small quantities to improve casting properties.

Beryllium

This metal is a carcinogen. It causes granuloma (a type of malignant tumor) in the lungs, liver, spleen and heart. Upon contact with beryllium, skin diseases develop and a severe weakening of the immune system is observed. In Russia, its use in dental alloys is prohibited.

How does metal-ceramics differ from other types of crowns?

In comparison with other types of orthopedic products, a metal-ceramic tooth crown is considered one of the best solutions in terms of biocompatibility, functionality and aesthetics. This type of crown is durable and reliable, and much cheaper than all-ceramic, zirconium and other types of products. An important feature of the designs is that they have a minimal list of contraindications and there are no restrictions on the age categories of patients.

Unique Features

The design features of metal-ceramic products allow them to be installed even in those patients who have more than half of their natural teeth destroyed. Perhaps this is due to:

  • a specific frame that minimizes the difference between the base and the ceramic part of the product;
  • features of the relief of the coating, which, like natural enamel, can refract streams of light.

The ceramics contain microscopic crystals that ensure the structural integrity of the structure.

Materials

Taking into account the biological characteristics and preferences of patients, orthopedists use different metal alloys to create a frame:

  • chromium-nickel. Easy to customize and low cost. It has a significant drawback - over time, the material oxidizes and a metallic taste appears in the mouth. The material can also provoke allergies;
  • cobalt-chromium. Practically does not irritate mucous membranes, the average biocompatibility is 36%. The material is characterized by strength and economy. Before making a prosthesis, it is advisable to perform a tolerance test, since the alloy can cause allergic reactions;
  • from noble metals: platinum, gold, palladium. This alloy does not oxidize, ideally follows the natural shape of the tooth and has high ductility. The only drawback is the high cost of the products.

Which of the materials will be best for a particular case can only be determined by a doctor after collecting an anamnesis and conducting diagnostic examinations.

Alloys in cermets

To make a metal-ceramic crown, the dental technician first makes a metal frame that exactly matches the contours of the tooth prepared for prosthetics. The frame is the most important part of the design of a metal-ceramic crown.

There is a saying: “the mouth is the beginning of the stomach, saliva is the first “stomach” juice.” Saliva is rich in a variety of enzymes. As a result of a chemical reaction, the metals that make up the alloy of the metal-ceramic prosthesis are “washed out” by saliva into the oral cavity in microdoses. Next, saliva with microdoses of metals is swallowed, absorbed through the gastrointestinal tract and enters the liver. This causes slow poisoning of the body.

The ceramic layer covering the outside surface of the metal frame is a good barrier to saliva and is an excellent insulating material. The teeth are isolated from the metal with high-strength cement, which completely protects your tooth from harmful factors, but metal is still present in the structure, and no one can guarantee that subtle biochemical reactions between your body and the metal frame do not occur.

There is no “best alloy” that suits everyone; patients have different sensitivities to certain elements. The determining factor here is the degree of corrosion. The fewer components of the alloy are dissolved, the less danger there is of a pathological reaction of the body to metal-ceramics. It follows from this that the alloy should contain a minimum of base components, because they are more susceptible to corrosion compared to noble metals.

Determination of the allergic effects of the alloy is carried out using tests on animals. Direct transfer of results to humans is not shown, however, it is possible to establish the allergic potential of the alloy.

Cost of crowns

To find out what costs await you when using metal-ceramic prosthetics, you should consider a number of factors:

  • complexity of the defect to be eliminated;
  • materials used to make an orthopedic product;
  • diagnostic and therapeutic procedures;
  • prosthesis manufacturing technologies;
  • doctor's qualifications.

Only after a thorough examination and diagnosis will a specialist be able to determine how much it will cost to install a crown. Depending on the material, prices vary between 4.5-17 thousand rubles. The cheapest products are made from domestic materials. Foreign-made alloys will cost more. And naturally, the most expensive are structures made of noble metals.

If the patient has temporary crowns installed, then the cost of each structure will be approximately 900-1200 rubles.

The Berezka clinic installs metal-ceramic prostheses made of various alloys. In the price list you can see the cost of products and choose the most suitable ones for yourself. You should not skimp on the health and attractiveness of your teeth. Contact our dentists, regardless of whether you need correction of already installed structures or prosthetics from scratch.

Aesthetic properties of metal ceramics

Metal-ceramic crowns have excellent aesthetic qualities. Modern technologies make it possible to achieve any shade of ceramic coating color.

In the 60s and 70s, there was a fashion for the so-called “Hollywood smile”, to create which metal-ceramic dentures with straight white teeth were made. Despite its external attractiveness, the “Hollywood smile” is unnatural, lifeless and, with rare exceptions, does not match the remaining teeth.

Increasingly, patients began to express wishes that artificial teeth would not differ from the preserved natural ones. But the possibilities of materials for the manufacture of metal-ceramic dentures were then very limited.

This led to the emergence of a number of research projects aimed at developing dyes, effect masses, opalescent porcelains, etc. A revolutionary step in the development of materials for creating natural aesthetics in dentures was the creation of the internal coloring technique, developed by one of the world's most famous dental technicians, Hitoshi Aoshima. The principle of this technique is that all the characteristic features of the tooth are not drawn with dyes on the surface of the metal-ceramic prosthesis, but are modeled from the inside.

Luster (glossy) porcelain was also developed. Research scientists have come to the conclusion that tooth enamel, in its shine, resembles the surface of a pearl. To imitate the natural shine of enamel, scientists have created a new technology for producing opalescent materials. The surface of luster porcelain, thanks to the ultra-fine structure of the particles, resembles the enamel of a natural tooth in its relief, ability to transmit light and color.

If the metal ceramics nevertheless turn black, then the reason for this may be trivial - the patient forgets to brush his teeth. If the lowest layer of ceramic, opaque, does not sufficiently dampen the metal frame and allow chromium ions to pass through (in the case of a cobalt-chromium alloy), then they give the accumulated plaque an unpleasant greenish tint. Individual oral hygiene is very important for everyone, and especially for those who have metal-ceramic dentures.

Caring for metal-ceramic crowns

Along with the fact that caring for artificial metal-ceramic teeth is quite simple, there are some rules that, if followed, can extend the service life of the products:

  • You need to brush your teeth at least twice a day. Movements should be vertical, directed towards the tooth edge from the gum;
  • The brush should have soft bristles. Any paste can be used according to the patient’s individual preferences;
  • You should not limit yourself to just brushing, since food remains remain in the interdental spaces. To remove them, you need to use dental floss;
  • After brushing, you should rinse your mouth with clean water and only then use an antiseptic mouthwash;
  • Lovers of coffee or other coloring foods and drinks, as well as smokers, are recommended to have their teeth professionally cleaned at least twice a year. Whitening pastes will not provide a positive effect in caring for metal ceramics, so home whitening is not advisable.

In addition to hygiene procedures, you also need to know that strong mechanical loads can lead to cracks and chips in the ceramic coating. Also, sudden temperature changes worsen the condition of the dentures, so it is not recommended to eat excessively hot or very cold food.

Prosthetics with metal-ceramics

Advantages of metal-ceramic prosthetics

The following facts speak in favor of the use of metal ceramics:

  • correspondence of artificial metal-ceramic teeth to natural ones in function and appearance
  • the possibility of prosthetics for both frontal and lateral teeth, included and end defects of the dentition, the ability to combine removable and non-removable metal-ceramic structures.
  • "hygienic" Microbial plaque settles less on metal-ceramic teeth than on natural teeth, which is especially important for patients with periodontitis.
  • durability. Today, metal ceramics are one of the most durable structures used in dentistry. If a metal-ceramic crown is made using modern materials and techniques, then its service life is on average from 10 (on a non-precious alloy) to 15 (on a gold-platinum alloy) years.
  • A properly made metal-ceramic crown will never cause unpleasant changes in the gums, such as bleeding, changes in color or contour.

Crown for one tooth

A metal-ceramic crown for one tooth is used to restore the upper part destroyed by caries or damaged by cracks and chips. Single denture structures differ in the method of fixation and materials of manufacture.

The choice of crown attachment method is carried out taking into account the degree of preservation of the tooth root:

  • if the roots are not damaged and more than 50% of the coronal part is preserved, then there is no need to use auxiliary structures for installation. The prosthesis is attached to a previously depulped, filled and ground tooth;
  • in case of complete destruction of the coronal part and satisfactory condition of the root system, the prosthesis is fixed by installing a pin. This is a rod that is installed in the root canal and cemented to increase stability;
  • in the complete absence of a unit in the dentition, the prosthesis is installed using the implantation technique. The artificial root ideally replaces the natural one in functionality and is a reliable support for the crown.

Regardless of the type of fixation, a very universal procedure is the installation of a single crown. It is made individually for each patient according to an impression and only after fitting and adjustment is fixed to the selected support.

Rating
( 1 rating, average 4 out of 5 )
Did you like the article? Share with friends:
For any suggestions regarding the site: [email protected]
Для любых предложений по сайту: [email protected]